Evaluation of the effect of different zirconia etching solutions on shear bond strength. A concise review

Authors

DOI:

https://doi.org/10.32828/y35tx094

Keywords:

Zirconia, Etching solutions, Shear bond, resin cement, hydrofluoric acid

Abstract

Aim: Different surface treatments were developed to enhance zirconia-resin cement bond strength. Conventional etching with hydrofluoric acid is not effective in enhancing bond strength, however, recent emerging acid etching formulations are thought to enhance zirconia-resin cement. The purpose of the current review is to clarify and summarize zirconia acid etching solutions that were tried to be used as a surface treatment, and to show its capability to enhance zirconia-resin cement bond strength. 

Materials and methods: PubMed and Google Scholar were searched for studies that investigated (zirconia etching) and (shear bond strength), and (zirconia etching solution), 11 studies were found, 6 of which matched the study criteria and were included in this review.

Conclusion: highly corrosive acids in high temperature and concentrations could enhance the shear bond strength of zirconia to resin cement.

Author Biographies

  • Ahmed Sleibi, College of Dentistry, Mustansiriyah University, Baghdad, Iraq

    Department of Conservative dentistry, Faculty of Dentistry

  • Abdul Rahman M Saleh, College of Dentistry, Ajman University, Ajman, United Arab Emirates

    Department of Clinical Sciences, College of Dentistry

References

References:

1) Kim SH, Cho SC, Lee MH, Kim HJ, Oh NS. Effect of 9% hydrofluoric acid gel hot-etching surface treatment on shear bond strength of resin cements to zirconia ceramics. Med 2022;58:1469.

2) Yu MK, Oh EJ, Lim MJ, Lee KW. Change of phase transformation and bond strength of Y-TZP with various hydrofluoric acid etching. Restor Dent Endod 2021;46(4): e54.

3) Borges GA, Sophr AM, De Goes MF, Sobrinho LC, Chan DC. Effect of etching and airborne particle abrasion on the microstructure of different dental ceramics. J. Prosthet. Dent. 2003; 89:479-488.

4) Janda R, Roulet JF, Wulf M, Tiller HJ. A new adhesive technology for all-ceramics. Dent. Mater 2003;19:567-573.

5)Thamrongananskul N, Busabok C. Poolthong S, Uo M, Tagami J. Dental zirconia can be etched by hydrofluoric acid. Dent. Mater 2014;33: 79-85.

6) Sadid-Zadeh R, Strazzella A, Li R, Makwoka S. Effect of zirconia etching solution on the shear bond strength between zirconia and resin cement. J Prosthet Dent;2021:126:693-697.

7) Kim HE, Lim MJ, Yu MK, Lee KW. Changes in bond strength and topography for Y-TZP etched with hydrofluoric acid depending on concentration and temperature conditions. Med 2020;56:568.

8) Colombo M, Gallo S, Padovan S, Chiesa M, Poggio C, Scribante A. Influence of different surface pretreatments on shear bond strength of an adhesive resin cement to various zirconia ceramics. J Mater 2020;13:652.

9) Yu MK, Lim MJ, Na NR, Lee KW. Effect of hydrofluoric acid-based etchant at an elevated temperature on the bond strength and surface topography of Y-TZP ceramics. Restor Dent Endod 2020;45:1.

10) Ansari S, Jahedmanesh N, Cascione D, Zafarnia P, Shah K C, Wu B M, Moshaverinia A. Effects of an etching solution on the adhesive properties and surface microhardness of zirconia dental ceramics. J Prosthet Dent 2018;120:447-453.

11) Sales A, Rodrigues SJ, Mahesh M, Ginjupalli K, Shetty T, Pai UY, et al. Effect of Different Surface Treatments on the Micro-Shear Bond Strength and Surface. Int J Dent 2022;1-12.

12) Seo SH, Kim JE, Nam NE, Moon HS. Effect of air abrasion, acid etching, and aging on the shear bond strength with resin cement to 3Y-TZP zirconia. J Mech Behav Biomed Mater. 2022;134:105348.

13) Carvalho RF, Rippe MP, Melo RM, Bottino MA, Souza RO. Resin bond strength to zirconia: effects of surface treatments and resin cements. Gen Dent 2019;67:71-7.

14) Saade J, Skienhe H, Ounsi HF, Matinlinna JP, Salameh Z. Evaluation of the effect of different surface treatments, aging and enzymatic degradation on zirconia-resin micro-shear bond strength. Clin Cosmet Investig Dent 2020;6:1-8.

15) Ban S. Chemical durability of high translucent dental zirconia. Dent Mater J. 2020;39:12-23.

16) Xia Y, Xu F, Chen L, Zhou X, Cao Y, Tong H. Effect of different surface zirconium oxide treatments on binding strength between zirconia and veneering ceramics. Zhong nan da xue xue bao. Yi xue ban= J Cent South Univ. Medical Sciences. 2019;44:53-8.

Downloads

Published

30.12.2024

How to Cite

Evaluation of the effect of different zirconia etching solutions on shear bond strength. A concise review. (2024). Mustansiria Dental Journal, 20(2), 200-205. https://doi.org/10.32828/y35tx094

Similar Articles

1-10 of 159

You may also start an advanced similarity search for this article.