Fracture strength and color stability of direct composite veneer using different materials

Authors

  • Mohammed Hamoudi Alsunboli Assistant lecture at College of Dentistry, AL-BAYAN University
  • Haider Hasan Jasim Assistant professor at college of dentistry , Al.Mustansiria University

DOI:

https://doi.org/10.32828/mdj.v18i1.916

Keywords:

Direct veneer and composite veneer. Color stability, fracture resistance

Abstract

Aim: The purpose of this study was to compare the fracture resistance and color stability of three different restoration materials: Nano composite, flowable composite, and Nanohybid composite.

Materials and Methods: 45 removed human maxillary premolar teeth for orthodontic treatment were chosen. The teeth were divided into three experimental groups, each consisting of fifteen teeth: Direct composite veneers constructed of Nano - composites were employed to fix the teeth in Group A. (Z350 XT, 3M, USA). Group B: Flowable composite was used to directly veneer teeth (G-aenial Universal flo GC, Japan). Group C: Direct composite veneers made of Nanohybid composite were used to reconstruct teeth (G-aenial GC, Japan). Each tooth in groups A, B, and C had a copyplast template made prior to preparation using a 1 mm thick vacuum-pressed polyethylene plastic template. Standard preparations (intra enamel) were made for all teeth in experimental groups using ceramic veneer set burs. By injecting flowable composite via a hole formed in a copyplast template, Group B is restored. In Groups A and C, the buccal third (Bucco-palatally) of the template was filled with restorative material using a plastic tool before being positioned on the tooth and squeezed until it made contact with the unprepared tooth surface. All specimens' baseline colors were assessed using a spectrophotometer (Vita Easyshade, Ivoclar VivadentAG, Schaan, Liechtenstin). After baseline color measurement, each group of laminate veneers were subjected to immersion solutions (Tea bags, Lipton). Each specimen's color values were once again measured with the same spectrophotometer,

 

and the color change values (ΔE) were computed. Using a universal testing equipment, the fracture strength was evaluated.

References

References

(1)bdul Khaliq, A. G., and I. I. Al-Rawi. Fracture strength of laminate veneers using different restorative materials and techniques (A comparative in vitro stuy) (2014).. Journal of Baghdad College of Dentistry. 26:1-8

(2)Acar O, Yilmaz B, Altintas SH, Chandrasekaran I, Johnston W. Color stability of CAD/CAM and nanocomposite resin materials. (2016) J Prosthet Dent; 115: 71-75.

(3)Akoglu, B., and D. Gemalmaz.. Fracture resistance of ceramic veneers with different preparation designs. Journal of prosthodontics (2011).: official journal of the American College of Prosthodontists 20:380-384

(4)Al kheraif A, Qasim S, Ramikrishnaiah R, Rehman I.. Effect of different beverages on color stability and degree of conversion of nano and microhybrid composites(2013). Dent Mater J; 32(2): 326-331.

(5)Alghazzawi TF1, Lemons J, Liu PR, Essig ME, Janowski GM. The failure load of CAD/CAM generated zirconia and glass-ceramic laminate veneers with different preparation designs(2012).. J Prosthet Dent; 108(6):386-393.

(6)Al-Qrimli, A., and A. Al-Shamma.). Comparative Evaluation of the Effect of Different Universal Adhesives and Bonding Techniques on the Marginal Gap of Class I Composite Restoration(2016 )(A SEM study), University of Baghdad.

(7) Anil K Tomer, Afnan Ajaz Raina, Faizan Bin Ayub, Akankshita Behera, Nitish Mittal, Sneha Vaidya, Midhun Ramachandran and Ashvin G John, Fracture strength of composite veneers using different restorative materials: A comparative in vitro study, International Journal of Applied Dental Sciences 2017; 3(4): 465-468.

(8)Archangelo CM, Rocha EP, Anchieta RB, Martin M, Freitas AC, Ko C, Cattaneo PM. Influence of buccal cusp reduction when using porcelain laminate veneers in premolars(2011).. A comparative study using 3-D finite element analysis. J Prosthodontic Research; 55: 221-227.

(9)Bagheri R, Burrow MF, Tyas M..Influence of food-simulating solutions and surface finish on susceptibility to staining of esthetic restorative materials(2005). J Dent; 33: 389-398.

(10)Batalocco G, Lee H, Ercoli C, Feng C, Malmstrom HFracture resistance of composite resin restorations and porcelain veneers in relation to residual tooth structure in fractured incisors.(2012).. Dental Traumatology 28: 75-80.

(11)Bindua M.G., Bhabani K. Satapathya, Harjeet S Jaggia, Alok R. Rayb Size-scale effects of silica on bis-GMA/TEGDMA based nanohybrid dental restorative composites(2013).. Composites Part B: Engineering October; (53): 92–102.

(12) Chandramouli MK. Componeers. Int J Prev Clin Dent Res 2017;4:232-4. .

(13)Cherukara GP, Davis GR, Seymour KG. Dentin exposure in tooth preparations for porcelain veneers(2005).: A pilot study. J Prosthet Dent; 94(5):414-420.

(14)De Munck, J. d., K. Van Landuyt, M. Peumans, A. Poitevin, P. Lambrechts, M. Braem, and B. Van Meerbeek.. A critical review of the durability of adhesion to tooth tissue(2005): methods and results. Journal of dental research 84:118-132.

(15)Dietschi D,Ardu S,Krejci I. A new shading concept based on natural tooth color applied to direct compsite restorations(2006)..Quintessence Int.;37:91-102.

(16)Dikova T, Abadjiev M, Balcheva M.). Clinical application of the contemporary nano-materials (part 1 – laboratory composites). J of IMAB,; 2:67-70.

(17)Er AU, Turker SB, Kocak A, Aktepe E). Effect of five staining solutions on the colour stabilityof two acrylics and three composite resins based provisional restorations.(2006. Eur J Prosthodont Restor Dent; 14: 121-125.

(18)Ertas E, Guler AU, Yucel AC, Koprulu H, Guler E.. Color stability of resin composites after immersion in different drinks(2006). Dent Mater J; 25: 371-376.

(19)Fahl N Jr, Ritter AV. Composite veneers: The directindirect technique revisited.J Esthet Restor Dent. 2021

(20)Fernando R, Andrade J, Sillas D. Fluorescence: Clinical Evaluation of New Composite Resins(2012).. QDT; ;35: 145-156.

(21)Friedman MJ. A 15-year review of porcelain veneer failure: a clinician’s observations. (1998). Compendium of Continuing Education in Dentistry; 19(6):625–8.

(22)Gale, M., and B. Darvell. Thermal cycling procedures for laboratory testing of dental restorations(1999).. Journal of dentistry 27:89-99.

(23)Gresnigt M, Özcan M. Fracture strength of direct versus indirect laminates with and without fiber application at the cementation interface(2007).. Dental Materials; 23:927-933.

(24)Gresnigt M.. Clinical and Laboratory Evaluation of Laminate Veneers(2011), chapter one: Introduction. Thesis, Department of Fixed and Removable Prosthodontics, University of Groningen, The Netherlands,.

(25)Gürel G.. Predictable, precise, and repeatable tooth preparation for porcelain laminate veneers(2003). Pract Proced Aesthet Dent.;15(1):17-26.

(26)Harleen Narula, Virinder Goyal, Kanika Gupta A comparative evaluation of fractural strength and marginal discrepancy of direct composite veneers using four different tooth preparation techniques (2019) : An in vitro studyJournal of Indian Society of Pedodontics and Preventive Dentistry 37(1):55

(27)Kaur P, Reena LP, Puneet. Nanocomposites - A step towards improved restorative dentistry(2011).. Ind J Dent Sci.; 4(3):28–31.

(28)Khatib D, Katamish H, Ibrahim ASFracture Load of Two CAD/CAM Ceramic Veneers with Different Preparation Designs. (2009).. Cairo Dental Journal; 25 (3), 425:432.

(29)Khatib D, Katamish H, Ibrahim AS. Fracture Load of Two CAD/CAM Ceramic Veneers with Different Preparation Designs(2009).. Cairo Dental Journal; 25 (3), 425:432.

(30)Kikuti WY, Chaves FO, Di Hipólito V, Rodrigues FP, D’Alpino PHP.. Fracture resistance of teeth restored with different resin based restorative systems(2012). Braz Oral Res; 26(3):275-81.

(31)Kournetas N, Chmkamakchi M, Kakaboura A, Rahiotis C, Gerstorfer GJMarginal and internal adaptation of class II Ormocer and hybrid resin composite restorations before and after load cycling. (2004).. Clin Oral Investig; 8: 123-129.

(32)Lin TM1, Liu PR, Ramp LC, Essig ME, Givan DA, Pan YH. Fracture resistance and marginal discrepancy of porcelain laminate veneers influenced by preparation design and restorative material in vitro(2012).. J Dent; 40(3):202-9.

(33)Magalhaes A, Siqueira P, Cardoco P, Souza J, Fonseca R et al. Influence of the resin cement color on the shade of porcelain veneers after accelerated artificial aging(2013)..Rev Odontol Bras Central; 21(6): 11-15.

(34) Mahesh Patel, Sangam Sangral & Jayaprakash Murugesan, Study on microstructure and mechanical properties of hybrid aluminium matrix composite with ZrO2 and Ni particle as reinforcement fabricated through FSP route Published online: 16 Sep 2022

(35)Malekipour M, Sharafi A, Kazei S, Khazaei S, Shirani F.).Comparison of color stability of a composite resin in different color media(2012. Dent Res J; 9(4): 441-446.

(36) Muñoz, M.; Luque-Martinez, I.; Hass, V.; Gutierrez, M.; Reis, A.; Loguercio, A. The sonic application of universal adhesives inself-etch mode improves their performance on enamel. Int. J. Adhes. Adhes. 2019, 88, 43–49.

(37)Mizrahi B. Porcelain Veneers: Techniques and precautions(2017).. International Dentistry SA; 9(6):6-16.

(38)Nogueira A, Della Bona A. The effect o a coupling medium on color and translucency of CAD-CAM ceramics(2013).. J of Dent; 41(3): 18-23.

(39)Omata Y, Uno S, Nakaoki Y et al. Staining of hybrid composites with coffee, oolong tea, or red wine. Dent Mater J 2006; 25: 125-131.

(40)Özcan M, Meşe A. Effect of Ultrasonic Versus Manual Cementation on the Fracture Strength of Resin Composite Laminates(2009).. Oper Dent; 34(4):437-442.

(41)Özcan M, Meşe A. Effect of Ultrasonic Versus Manual Cementation on the Fracture Strength of Resin Composite Laminates(2009).. Oper Dent; 34(4):437-442.

(42) Panteqi S, Meto A, Simeon O. Componeers vs porcelains. Int J Sci Res 2018;7:1680-2.

(43)Rao YM, Srilakshmi V, Vinayagam KK, Narayanan LL..An evaluation of the color stability of tooth colored restorative materials after bleaching using CIE LAB color technique(2009). Indian J Dent Res; 20: 60-64.

(44)Rezvani M.B., Basir M.B.,Mollavedi F., Moradi Z., Sobout A. Comparison of the Effect of Direct and Indirect Composite Resin Restorations on the Fracture Resistance of Maxillary Premolars(2012).: An In Vitro Study. J. Dent school; 29(5):299-35.

(45))Roberson M, Heyman H, Swift E. Sturtevant’s art and science of operative dentistry. 4th edition. Mosby(2002)... Ch4-P190-210.

(46)Rosentritt M, Sawaljanow A, Behr M, Kolbeck C, Preis V. Effect of tooth brush abrasion and thermo-mechanical loading on direct and indirect veneer restorations(2015).. Clin Oral Invest; 19: 53-60.

(47)Rosentritt M, Sawaljanow A, Behr M, Kolbeck C, Preis V. Effect of tooth brush abrasion and thermo-mechanical loading on direct and indirect veneer restorations(2015).. Clin Oral Invest; 19: 53-60.

(48)Rueggeberg, F.. Substrate for adhesion testing to tooth structure—Review of the literature: A report of the ASC MD156 Task Group on Test methods for the adhesion of restorative materials Accredited standards committee MD156 for dental materials and devices(1991). Dental Materials 7:2-10.

(49)Shereen m el sayed,* rasha ramadan basheer ** and sherif fayez ahmed bahgat.. Color stability and fracture resistance of laminate veneers using different restorative materials and techniques(2016). Vol. 62, 1:15, April,.

(50)Silva Leite M, Silva F, Meireles S, Duarte R, Andrade A. The effect of drinks on color stability and surface roughness of nanocomposites(2014).. Europ J Dent; 8(3): 330-336.

(51)Singh K, Suvarna S, Agnihotri Y, Sahoo S, Kumar PColor stability of aesthetic restorative materials after exposure to commonly consumed beverages. (2015).: A systematic review of literature. Eur J Prostho; 2(1): 15-22.

(52)Stawarczyk B, Sener B, Trottmann A, Roos M, Ozcan M, Hammerle C. Discoloration of manually fabricated resins and industrially fabricated CAD blocks versus glass-ceramic: effect of storage media, duration, and subsequent polishing(2012).. Dent Mater J; 31(3):377-383.

(53)Touati B., Miara P.,Nathanson D..Esthetic Dentistry and Ceramic restorations.United Kingdom:Martin Dunitz Ltd. (1999)

(54)Turgut S, Bagis B. Color stability of laminate veneers(2011).: An in vitro study. J of Dent; 39: 57-64.

(55)Turgut S, Bagis B. Color stability of laminate veneers: An in vitro study. J of Dent 2011; 39: 57-64.

Turkaslan S, Tezvergil-Mutluay A, Bagis B, Vallittu Pk, Lassila LV.). Effect of fiber-reinforced composites on the failure load and failure mode of composite veneers. (2009 Dent Mater J Sep; 28(5):530-6.

(56)Turkaslan S, Tezvergil-Mutluay A, Bagis B, Vallittu Pk, Lassila LV.. Effect of fiber-reinforced composites on the failure load and failure mode of composite veneers(2009). Dent Mater J Sep; 28(5):530-6.

(57)Um CM, Ruyter IE. Staining of resin based veneering material with coffee and tea(1991).. Quint Int; 22:337-386.

(58)Vichi A, Ferrari M, Davidson CM.). Color and opacity variations in three different resin based composite products after water aging(2004. Dent Mater J; 20: 530-534.

(59) Wiesse, P.; Silva-Sousa, Y.; Pereira, R.; Estrela, C.; Domingues, L.; Pécora, J.D.; Sousa-Neto, M.D.d. Effect of ultrasonic and sonic activation of root canal sealers on the push-out bond strength and interfacial adaptation to root canal dentine. Int. Endod. J. 2018, 51, 102–111.

Downloads

Published

16.10.2022

How to Cite

Hamoudi Alsunboli , M. ., & Hasan Jasim , H. . (2022). Fracture strength and color stability of direct composite veneer using different materials. Mustansiria Dental Journal, 18(1), 135–150. https://doi.org/10.32828/mdj.v18i1.916